Brand Name : Zhonggong Special Metallurgy
Model Number : GH136 Alloy
Place of Origin : China
MOQ : 100KG
Price : Price is negotiated based on the required specifications and quantity
Payment Terms : Payment Terms: Mainly T/T.. L/C, D/A, D/P,
Supply Ability : 5000 tons per month
Delivery Time : 5-8 working days, depending on the parameters required for negotiation
Packaging Details : Standard export packaging, or packaging as required
Density : ~8.8 g/cm³ (0.317 lb/in³)
Melting Point : ~1300-1400°C (2370-2550°F)
Tensile Strength : ~900 MPa (130 ksi)
Yield Strength : ~700 MPa (102 ksi)
Elongation : ~15%
Thermal Conductivity : ~13 W/m·K (9 BTU·in/hr·ft²·°F)
Modulus of Elasticity : ~210 GPa (30 x 10³ ksi)
Corrosion Resistance : Good oxidation and corrosion resistance at high temperatures
Certification : ISO Certificate
GH136 Alloy is a high-performance nickel-based superalloy engineered for superior strength and oxidation resistance at elevated temperatures. This alloy is designed to perform reliably in extreme environments, making it suitable for demanding applications in aerospace and high-temperature industrial processes.
Key Properties and Features:
GH136 Alloy’s combination of high strength, oxidation resistance, and thermal stability ensures it is a reliable choice for advanced engineering applications demanding exceptional performance under extreme conditions.
Here’s a composition table for GH136 Alloy:
Element | Composition Range (%) |
---|---|
Nickel (Ni) | 60.0 - 65.0 |
Chromium (Cr) | 14.0 - 16.0 |
Cobalt (Co) | 8.0 - 10.0 |
Molybdenum (Mo) | 3.0 - 5.0 |
Iron (Fe) | ≤ 6.0 |
Titanium (Ti) | 1.0 - 2.0 |
Aluminum (Al) | 1.0 - 2.0 |
Carbon (C) | ≤ 0.10 |
Manganese (Mn) | ≤ 0.5 |
Silicon (Si) | ≤ 0.5 |
Sulfur (S) | ≤ 0.01 |
These values provide general guidelines. For precise specifications or applications, consult specific standards or suppliers.
![]() |
GH136 Alloy is a nickel-based superalloy with high strength and excellent oxidation resistance at elevated temperatures Images |